| Abrasion Tester Type APG (2) |
| |
Functioning:
A paper strip of 10 m length is continuously pulled over a painted specimen. The
paper strip is pressed on the specimen by a defined weight. The result of the
test is the amount of paper strip in cm necessary until there is no longer paint
on the specimen.
Results:
Highly resistance against abrasion - length of the paper strip necessary more
than 100 cm. Normal resistance - paper strip length less than 10 cm. |
 |
|